General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.42 g/cm³ Show Supplier Material materials with Densidad of 1.42 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard |
---|---|---|---|
Elongación | 1.1 % Show Supplier Material materials with Elongación of 1.1 % | dry | ISO 527-1/-2 |
Módulo elástico | 9 GPa Show Supplier Material materials with Módulo elástico of 9 GPa | dry | ISO 527-1/-2 |
Resistencia a la tracción | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
3.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |
Conductividad térmica | 2.1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 2.1 W/(m·K) | dry | ASTM E1461 | through plane |
14.0 W/(m·K) Show Supplier Material materials with Conductividad térmica of 14.0 W/(m·K) | dry | ASTM E1461 | in plane | |
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+07 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+07 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 10000 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | LED Headlight Lighting Modules and Lensholders, Cover Electric Control Unit | |
Fillers | 15% Glass Fiber |