General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 3 % Show Supplier Material materials with Absorción de agua of 3 % | dry | ISO 62 | at 23°C after 24h |
10.5 % Show Supplier Material materials with Absorción de agua of 10.5 % | dry | Sim. to ISO 62 | ||
Densidad | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.9 % Show Supplier Material materials with Moisture absorption of 2.9 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 13 % Show Supplier Material materials with Elongación of 13 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 125 MPa Show Supplier Material materials with Flexural yield strength of 125 MPa | dry | ISO 178 | |
Módulo de flexión | 3.1 GPa Show Supplier Material materials with Módulo de flexión of 3.1 GPa | dry | ISO 178 | |
Módulo elástico | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | 0.75 mm | UL746B | ||
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | Aramid Fiber |