General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.5 g/cm³ Show Supplier Material materials with Densidad of 1.5 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 1.7 % Show Supplier Material materials with Elongación of 1.7 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | |
Módulo de flexión | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | dry | ISO 178 | |
Módulo elástico | 11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 4.6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.6 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.7e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6.6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 235 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 235 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 319 °C Show Supplier Material materials with Temperatura de fusión of 319 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.7 [-] Show Supplier Material materials with Constante dieléctrica of 3.7 [-] | dry | IEC 60250 | 5GHz |
3.74 [-] Show Supplier Material materials with Constante dieléctrica of 3.74 [-] | dry | IEC 60250 | 1GHz | |
3.75 [-] Show Supplier Material materials with Constante dieléctrica of 3.75 [-] | conditioned | IEC 60250 | 5GHz | |
3.8 [-] Show Supplier Material materials with Constante dieléctrica of 3.8 [-] | conditioned | IEC 60250 | 1GHz | |
Factor de disipación | 109 [-] Show Supplier Material materials with Factor de disipación of 109 [-] | dry | IEC 60250 | 5GHz |
137 [-] Show Supplier Material materials with Factor de disipación of 137 [-] | dry | IEC 60250 | 1GHz | |
140 [-] Show Supplier Material materials with Factor de disipación of 140 [-] | conditioned | IEC 60250 | 5GHz | |
170 [-] Show Supplier Material materials with Factor de disipación of 170 [-] | conditioned | IEC 60250 | 1GHz |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 35% Glass Fiber |