General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.06 % Show Supplier Material materials with Absorción de agua of 0.06 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2 % Show Supplier Material materials with Elongación of 2 % | dry | ISO 527-1/-2 |
9 % Show Supplier Material materials with Elongación of 9 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 90 MPa Show Supplier Material materials with Flexural yield strength of 90 MPa | dry | ISO 178 | |
120 °C | 12 MPa Show Supplier Material materials with Flexural yield strength of 12 MPa | dry | ISO 178 | |
160 °C | 8.5 MPa Show Supplier Material materials with Flexural yield strength of 8.5 MPa | dry | ISO 178 | |
200 °C | 7 MPa Show Supplier Material materials with Flexural yield strength of 7 MPa | dry | ISO 178 | |
Módulo de flexión | 2.7 GPa Show Supplier Material materials with Módulo de flexión of 2.7 GPa | dry | ISO 178 | |
120 °C | 0.36 GPa Show Supplier Material materials with Módulo de flexión of 0.36 GPa | dry | ISO 178 | |
160 °C | 0.24 GPa Show Supplier Material materials with Módulo de flexión of 0.24 GPa | dry | ISO 178 | |
200 °C | 0.2 GPa Show Supplier Material materials with Módulo de flexión of 0.2 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 3.3 GPa Show Supplier Material materials with Módulo elástico of 3.3 GPa | dry | ISO 527-1/-2 |
2.9 GPa Show Supplier Material materials with Módulo elástico of 2.9 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | -40 °C | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 |
60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 20 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | parallel, above Tg | ||
1.4e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.4e-06 1/K | dry | ISO 11359-1/-2 | normal, above Tg | ||
Inflamabilidad | V-2 | dry | IEC 60695-11-10 | ||
Temperatura de flexión bajo carga | 102 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 102 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 280 °C Show Supplier Material materials with Temperatura de fusión of 280 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 90 °C Show Supplier Material materials with Temperatura de transición del vidrio of 90 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 [-] | dry | IEC 60250 | 5GHz |
Factor de disipación | 23 [-] Show Supplier Material materials with Factor de disipación of 23 [-] | dry | IEC 60250 | 5GHz |
Rigidez dieléctrica | 41 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 41 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.2 % Show Supplier Material materials with Contracción of 1.2 % | dry | ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 300 °C | 24.6 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24.6 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 300 °C | 21.7 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 21.7 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|