General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.7 g/cm³ Show Supplier Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 55 - 65 % Show Supplier Material materials with Elongación of 55 - 65 % |
Estricción | 23.0 °C | 65 - 75 % Show Supplier Material materials with Estricción of 65 - 75 % |
Límite elástico Rp 0,2 | 23.0 °C | 610 - 720 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 610 - 720 MPa |
Resistencia a la tracción | 23.0 °C | 980 - 1120 MPa Show Supplier Material materials with Resistencia a la tracción of 980 - 1120 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. | |
Cromo | 16 - 20 % Show Supplier Material materials with Cromo of 16 - 20 % | ||
Hierro | Balance | ||
Manganeso | 12 - 16 % Show Supplier Material materials with Manganeso of 12 - 16 % | ||
Molibdeno | 2.5 - 4.2 % Show Supplier Material materials with Molibdeno of 2.5 - 4.2 % | ||
Niobio | 0.25 % Show Supplier Material materials with Niobio of 0.25 % | max. | |
Nitrógeno | 0.75 - 1 % Show Supplier Material materials with Nitrógeno of 0.75 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | The Ni-free steel grade P 2000 shows excellent biocompatibility and will be used mainly in contact with the human body, for the production of spectacle frames, watch cases and jewellery and after biological evaluation for the production of prosthesis for orthopaedics, bone screws and plates for osteosynthesis and high-strength wire for orthodontia. Additional applications result inevitably in cases where corrosion resistance, reliability and a high fa-tigue resistance are required. Examples are ultra high strength screws, nuts and bolts for the fastener industry. |