General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.51 g/cm³ Show Supplier Material materials with Densidad of 4.51 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 170 [-] Show Supplier Material materials with Dureza Brinell of 170 [-] | max. |
Elongación A50 | 23.0 °C | 18 % Show Supplier Material materials with Elongación A50 of 18 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 345 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 345 MPa | min. |
Módulo elástico | 23.0 °C | 105 GPa Show Supplier Material materials with Módulo elástico of 105 GPa | |
Resistencia a la tracción | 23.0 °C | 480 MPa Show Supplier Material materials with Resistencia a la tracción of 480 MPa | min |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 5.2E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.2E-7 Ω·m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. | |
Hidrógeno | 0.02 % Show Supplier Material materials with Hidrógeno of 0.02 % | max. | |
Hierro | 0.03 % Show Supplier Material materials with Hierro of 0.03 % | max. | |
Manganeso | 0.2 - 0.4 % Show Supplier Material materials with Manganeso of 0.2 - 0.4 % | ||
Nitrógeno | 0.03 % Show Supplier Material materials with Nitrógeno of 0.03 % | max. | |
Níquel | 0.6 - 0.9 % Show Supplier Material materials with Níquel of 0.6 - 0.9 % | ||
Otro | 0.4 % Show Supplier Material materials with Otro of 0.4 % | total | |
Oxígeno | 0.25 % Show Supplier Material materials with Oxígeno of 0.25 % | max. | |
Titanio | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Ti Gr 12 semi-finished products are used in some areas, but the material is mainly used in the chemical industry and in the manufacture of pressure vessels. | |
Corrosion properties | Titanium Gr.12 offers excellent corrosion resistance to acids as well as very good resistance to crevice corrosion in hot brines. Due to the higher strength, Titanium Gr.12 can be used with a thinner wall thickness than Titanium Gr.2 or Titanium Gr.7 under the same conditions. | |
Other | We are pleased to offer you powder for 3D printing made of Titan Grade 12 / 3.7105 / UNS N53400 |