Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7 g/cm³ Show Supplier Material materials with Densidad of 7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Dureza Brinell of 270 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. | |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. | |
Cobre | 0.11 % Show Supplier Material materials with Cobre of 0.11 % | max. | |
Cromo | 21 - 23 % Show Supplier Material materials with Cromo of 21 - 23 % | ||
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. | |
Hierro | Balance | ||
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. | |
Nitrógeno | 0.1 - 0.22 % Show Supplier Material materials with Nitrógeno of 0.1 - 0.22 % | ||
Níquel | 2.5 - 3.5 % Show Supplier Material materials with Níquel of 2.5 - 3.5 % | ||
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | 1.4462 is used mainly in sector of chemical industry, petrochemical industry, offshore, sea water lines, sea water desalination plants, nuclear engineering, paper and pulp industry. |