Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Ti 6Al-6V-2Sn
Titanium 6-6-2 is a heat treatable high strength titanium alloy with lower toughness and ductility than Titanium 6Al/4V. Titanium 6-6-2 has a similar machinability to Austenitic steel , easily welded providing precautions are taken to shield against Oxygen, Hydrogen and Nitrogen contaminants
Los datos sobre este material han sido proporcionados por Hempel Special Metals.
All categories
Technological properties
Property | ||
---|---|---|
Application areas | Ordinance components Airframe Rocket case applications Pressure canisters |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.