Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Hastelloy X / 2.4665
The nickel-chromium-iron-molybdenum alloy exhibits very good strength and oxidation resistance up to temperatures of 1200°C. The molybdenum content results in a high strength in a solid solution alloy. The solidification of the matrix caused by the molybdenum content results in high strength in a solid solution alloy.
Los datos sobre este material han sido proporcionados por Hempel Special Metals.
All categories
General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.22 g/cm³ Show Supplier Material materials with Densidad of 8.22 g/cm³ |
Technological properties
Property | ||
---|---|---|
Application areas | The material is used in gas turbines, industrial furnaces, heat treatment plants and nuclear technology. |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.