General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.81 g/cm³ Show Supplier Material materials with Densidad of 7.81 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -40.0 °C | 35 J Show Supplier Material materials with Charpy impact energy, V-notch of 35 J | min. |
23.0 °C | 80 J Show Supplier Material materials with Charpy impact energy, V-notch of 80 J | min. | |
Dureza Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Dureza Brinell of 270 [-] | max. |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | min. |
Estricción | 23.0 °C | 45 % Show Supplier Material materials with Estricción of 45 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 550 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 550 MPa | min. |
Módulo elástico | 23.0 °C | 199 GPa Show Supplier Material materials with Módulo elástico of 199 GPa | |
Resistencia a la tracción | 23.0 °C | 750 MPa Show Supplier Material materials with Resistencia a la tracción of 750 MPa | min. |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 33 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 33 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | max. | |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. | |
Cobre | 0.5 - 1 % Show Supplier Material materials with Cobre of 0.5 - 1 % | ||
Cromo | 24 - 26 % Show Supplier Material materials with Cromo of 24 - 26 % | ||
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. | |
Hierro | Balance | ||
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. | |
Molibdeno | 3 - 4 % Show Supplier Material materials with Molibdeno of 3 - 4 % | ||
Nitrógeno | 0.2 - 0.3 % Show Supplier Material materials with Nitrógeno of 0.2 - 0.3 % | ||
Níquel | 6 - 8 % Show Supplier Material materials with Níquel of 6 - 8 % | ||
Silicona | 0.01 % Show Supplier Material materials with Silicona of 0.01 % | max. | |
Wolframio | 0.5 - 1 % Show Supplier Material materials with Wolframio of 0.5 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Providing higher strengths than both austenitic and 22% Cr Duplex Stainless Steels UNS S32760 (F55) is suited to a variety of applications in industries such as Oil & Gas, CPI(Chemical Processing Industries), and Marine environments. | |
Corrosion properties | Super Duplex S32760/ F55 , Super Duplex Alloy UNS S32760 (F55 / 1.4501) has excellent resistance Pitting and Crevice Corrosion in seawater at elevated temperatures, supplied with a PREN 40<( Pitting Resistance Eqv) . Excellent resistance to SCC ( Stress Corrosion Cracking) in Sour and Chloride environments | |
Other | The material comes with a 3.1 certification. 3.2 certification are available with surcharge. |