General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1435 - 1445 °C Show Supplier Material materials with Temperatura de fusión of 1435 - 1445 °C |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % |
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % |
Cobre | 0.25 % Show Supplier Material materials with Cobre of 0.25 % |
Hierro | 0.04 % Show Supplier Material materials with Hierro of 0.04 % |
Magnesio | 0.15 % Show Supplier Material materials with Magnesio of 0.15 % |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % |
Níquel | 90 % Show Supplier Material materials with Níquel of 90 % |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 201 is commonly used in food industry, but it is also in used vessels up to 600°C and sodium hydroxide evaporators up to 450°C. Alloy 201 is also often used in vessels for production of flour, hydrochloric acid or vinylchloride monomer. | |
Welding | Filler metal (for welding with 2.4066/2.4068) |