General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.61 g/cm³ Show Supplier Material materials with Densidad of 8.61 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia al choque, ensayo Charpy entallado | -96.0 °C | 1200 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 1200 kJ/m² | min. |
23.0 °C | 1500 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 1500 kJ/m² | min. | |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1355 - 1400 °C Show Supplier Material materials with Temperatura de fusión of 1355 - 1400 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 5E-3 % Show Supplier Material materials with Azufre of 5E-3 % | max. |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % | max. |
Cobalto | 2.5 % Show Supplier Material materials with Cobalto of 2.5 % | max. |
Cromo | 20 - 22.5 % Show Supplier Material materials with Cromo of 20 - 22.5 % | |
Hierro | 2 - 6 % Show Supplier Material materials with Hierro of 2 - 6 % | |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. |
Molibdeno | 12.5 - 14.5 % Show Supplier Material materials with Molibdeno of 12.5 - 14.5 % | |
Níquel | 50 - 63 % Show Supplier Material materials with Níquel of 50 - 63 % | |
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % | max. |
Vanadio | 0.35 % Show Supplier Material materials with Vanadio of 0.35 % | max. |
Wolframio | 2.5 - 3.5 % Show Supplier Material materials with Wolframio of 2.5 - 3.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 22 is used in the petrochemical and chemical industry. 2.4602 is a common material when it comes to contact with hot, contaminated mineral acids, solutions or seawater. It is used also in bleaching containers (such as in the pulp and paper industry) and acetic acid production in a reactor. Alloy 22 also occurs in components with sour gas applications. | |
Corrosion properties | Alloy C22 is very resistant to many corrosive media under oxidizing and reducing conditions. It is, for example, resistant to: | |
Welding | Welding Rod (WIG) 2.4635 |