General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.6 g/cm³ Show Supplier Material materials with Densidad of 8.6 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia al choque, ensayo Charpy entallado | -196.0 °C | 2000 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2000 kJ/m² | min. |
23.0 °C | 2250 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2250 kJ/m² | min. | |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.1 - 0.4 % Show Supplier Material materials with Aluminio of 0.1 - 0.4 % | ||
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. | |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % | max. | |
Cobalto | 0.3 % Show Supplier Material materials with Cobalto of 0.3 % | max. | |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | max. | |
Cromo | 22 - 24 % Show Supplier Material materials with Cromo of 22 - 24 % | ||
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. | |
Hierro | 1.5 % Show Supplier Material materials with Hierro of 1.5 % | max. | |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. | |
Molibdeno | 15 - 16 % Show Supplier Material materials with Molibdeno of 15 - 16 % | ||
Níquel | Balance | ||
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 59 is used for: environmental technology, chemical industry (chemical processes with oxidating and reducing acids, resistance against damp chloric gas) and solid waste incinerators. Predominantly 2.4605 is used for chemical industry, pulp and paper industry and and flue gas desulfurization plants. | |
Other | Alloy 59 is stated in BAM-List (Hazardous Materials Transportation). |