General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 1500 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 1500 kJ/m² | max. |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1330 - 1380 °C Show Supplier Material materials with Temperatura de fusión of 1330 - 1380 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.6 - 1.5 % Show Supplier Material materials with Aluminio of 0.6 - 1.5 % | |
Azufre | 8E-3 % Show Supplier Material materials with Azufre of 8E-3 % | max. |
Boro | 6E-3 % Show Supplier Material materials with Boro of 6E-3 % | max. |
Carbono | 0.05 - 1 % Show Supplier Material materials with Carbono of 0.05 - 1 % | |
Cobalto | 10 - 13 % Show Supplier Material materials with Cobalto of 10 - 13 % | |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | max. |
Cromo | 20 - 23 % Show Supplier Material materials with Cromo of 20 - 23 % | |
Fósforo | 0.01 % Show Supplier Material materials with Fósforo of 0.01 % | max. |
Hierro | 2 % Show Supplier Material materials with Hierro of 2 % | max. |
Manganeso | 0.7 % Show Supplier Material materials with Manganeso of 0.7 % | max. |
Molibdeno | 8 - 10 % Show Supplier Material materials with Molibdeno of 8 - 10 % | |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % | max. |
Titanio | 0.02 - 0.5 % Show Supplier Material materials with Titanio of 0.02 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 617 is applied at high temperatures. Alloy 617 is used in air heaters, furnace components, beam pipes or high-temperature heat exchangers as well as in gas turbines and combustion chambers. | |
Welding | Welding Rods: FM 617- 2.4627 Wire Electrodes: Covered Rod Electrodes: |