General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.9 g/cm³ Show Supplier Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 690 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 690 kJ/m² |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 1.8 - 2.4 % Show Supplier Material materials with Aluminio of 1.8 - 2.4 % | ||
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | max. | |
Carbono | 0.15 - 0.25 % Show Supplier Material materials with Carbono of 0.15 - 0.25 % | ||
Circonio | 0.01 % Show Supplier Material materials with Circonio of 0.01 % | ||
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % | max. | |
Cromo | 24 - 26 % Show Supplier Material materials with Cromo of 24 - 26 % | ||
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. | |
Hierro | 8 - 11 % Show Supplier Material materials with Hierro of 8 - 11 % | ||
Iterbio | 0.05 - 0.12 % Show Supplier Material materials with Iterbio of 0.05 - 0.12 % | ||
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. | |
Níquel | Balance | ||
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. | |
Titanio | 0.1 - 0.2 % Show Supplier Material materials with Titanio of 0.1 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 602 is versatile. Typical applications of Alloy 602CA are, i.e.: | |
Welding | Alloy 602CA can be welded using 2.4649 and DIN EN ISO 18274: S Ni 6025 as filler metal Covered electrodes: |