General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.51 g/cm³ Show Supplier Material materials with Densidad of 4.51 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación A50 | 23.0 °C | 15 % Show Supplier Material materials with Elongación A50 of 15 % | min., Annealed, specification values (ASTM F67) |
Límite elástico Rp 0,2 | 23.0 °C | 483 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 483 MPa | min., Annealed, specification values (ASTM F67) |
Resistencia a la tracción | 23.0 °C | 550 MPa Show Supplier Material materials with Resistencia a la tracción of 550 MPa | min., Annealed, specification values (ASTM F67) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % |
Hidrógeno | 0.02 % Show Supplier Material materials with Hidrógeno of 0.02 % |
Hierro | 0.3 % Show Supplier Material materials with Hierro of 0.3 % |
Nitrógeno | 0.03 % Show Supplier Material materials with Nitrógeno of 0.03 % |
Oxígeno | 0.25 % Show Supplier Material materials with Oxígeno of 0.25 % |
Titanio | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Ti Gr.4 is used in the chemical industry, aviation and aerospace. Due to its very good biocompatibility, it is also used in medicine. |