General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.43 g/cm³ Show Supplier Material materials with Densidad of 4.43 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 15 % Show Supplier Material materials with Elongación A50 of 15 % |
Hardness, Rockwell | 23.0 °C | 34 [-] Show Supplier Material materials with Hardness, Rockwell of 34 [-] |
Límite elástico Rp 0,2 | 23.0 °C | 880 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 880 MPa |
Resistencia a la tracción | 23.0 °C | 950 MPa Show Supplier Material materials with Resistencia a la tracción of 950 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1650 °C Show Supplier Material materials with Temperatura de fusión of 1650 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 5.5 - 6.75 % Show Supplier Material materials with Aluminio of 5.5 - 6.75 % | |
Hidrógeno | 0.02 % Show Supplier Material materials with Hidrógeno of 0.02 % | max. |
Titanio | 88.74 - 91 % Show Supplier Material materials with Titanio of 88.74 - 91 % | |
Vanadio | 3.5 - 4.5 % Show Supplier Material materials with Vanadio of 3.5 - 4.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Titanium Grade 5 is found as most used alloy in many areas again. Thus, for example in: | |
Welding | As filler for titanium grade 5 titanium bare wire of the same group can be used. |