General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.43 g/cm³ Show Supplier Material materials with Densidad of 4.43 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación A50 | 23.0 °C | 10 % Show Supplier Material materials with Elongación A50 of 10 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 780 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 780 MPa | |
Resistencia a la tracción | 23.0 °C | 860 MPa Show Supplier Material materials with Resistencia a la tracción of 860 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 5.5 - 6.5 % Show Supplier Material materials with Aluminio of 5.5 - 6.5 % | ||
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. | |
Hidrógeno | 0.01 % Show Supplier Material materials with Hidrógeno of 0.01 % | max. | |
Hierro | 0.25 % Show Supplier Material materials with Hierro of 0.25 % | max. | |
Nitrógeno | 0.05 % Show Supplier Material materials with Nitrógeno of 0.05 % | max. | |
Titanio | Balance | ||
Vanadio | 3.5 - 4.5 % Show Supplier Material materials with Vanadio of 3.5 - 4.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Titanium Grade 23 ELI is found as most used alloy in medical industry for shoulder implants, hip-balls osteosyntheses, bone screws, bone plates, marrow-nails, spinalsystems, dental implants and tools. It's used also for: |