General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.51 g/cm³ Show Supplier Material materials with Densidad of 4.51 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 830 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 830 kJ/m² |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1670 °C Show Supplier Material materials with Temperatura de fusión of 1670 °C |
Chemical properties
Property | Value |
---|---|
Carbono | 0.06 % Show Supplier Material materials with Carbono of 0.06 % |
Hidrógeno | 0.01 % Show Supplier Material materials with Hidrógeno of 0.01 % |
Hierro | 0.25 % Show Supplier Material materials with Hierro of 0.25 % |
Nitrógeno | 0.05 % Show Supplier Material materials with Nitrógeno of 0.05 % |
Oxígeno | 0.18 % Show Supplier Material materials with Oxígeno of 0.18 % |
Plomo | 0.12 - 0.2 % Show Supplier Material materials with Plomo of 0.12 - 0.2 % |
Titanio | 99.3 % Show Supplier Material materials with Titanio of 99.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Titanium Grade 7 is preferably used in chemical plants. | |
Welding | As filler material for titanium grade 7 bare wire of the same titanium group should be used |