Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 16 % Show Supplier Material materials with Elongación of 16 % | min. |
Resistencia a la tracción | 23.0 °C | 750 - 897 MPa Show Supplier Material materials with Resistencia a la tracción of 750 - 897 MPa | min.:ISO 5832-12 and max.: ASTM F1537 |
Chemical properties
Property | Value |
---|---|
Carbono | 0.35 % Show Supplier Material materials with Carbono of 0.35 % |
Cobalto | Balance |
Cromo | 26 - 30 % Show Supplier Material materials with Cromo of 26 - 30 % |
Hierro | 0.75 % Show Supplier Material materials with Hierro of 0.75 % |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 5 - 7 % Show Supplier Material materials with Molibdeno of 5 - 7 % |
Nitrógeno | 0.25 % Show Supplier Material materials with Nitrógeno of 0.25 % |
Níquel | 1 % Show Supplier Material materials with Níquel of 1 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Joint replacement for hip knee, shoulder etc. marrow-nails and dental application. This material can also be used for watch cases as it has an outstanding polishing ability and corrosion resistance. |