General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.15 g/cm³ Show Supplier Material materials with Densidad of 8.15 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 130 [-] Show Supplier Material materials with Dureza Brinell of 130 [-] | Annealed, Descaled |
Elongación A50 | 23.0 °C | 40 % Show Supplier Material materials with Elongación A50 of 40 % | min., Annealed, Descaled |
Límite elástico Rp 0,2 | 23.0 °C | 248 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 248 MPa | Annealed, Descaled |
Resistencia a la tracción | 23.0 °C | 490 MPa Show Supplier Material materials with Resistencia a la tracción of 490 MPa | Annealed, Descaled |
Chemical properties
Property | Value |
---|---|
Hierro | Balance |
Níquel | 42 % Show Supplier Material materials with Níquel of 42 % |
Technological properties
Property | ||
---|---|---|
Application areas | Invar 42 is used mainly in: |