General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 6.51 g/cm³ Show Supplier Material materials with Densidad of 6.51 g/cm³ |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1852 °C Show Supplier Material materials with Temperatura de fusión of 1852 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 0.05 % Show Supplier Material materials with Carbono of 0.05 % | max. |
Circonio | 99.2 % Show Supplier Material materials with Circonio of 99.2 % | min., Zr+Hf |
Cromo | 0.2 % Show Supplier Material materials with Cromo of 0.2 % | max., Cr + Fe |
Hafmio | 4.5 % Show Supplier Material materials with Hafmio of 4.5 % | max. |
Hidrógeno | 5E-3 % Show Supplier Material materials with Hidrógeno of 5E-3 % | max. |
Hierro | 0.2 % Show Supplier Material materials with Hierro of 0.2 % | max., Cr + Fe |
Nitrógeno | 0.03 % Show Supplier Material materials with Nitrógeno of 0.03 % | max. |
Oxígeno | 0.16 % Show Supplier Material materials with Oxígeno of 0.16 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Zr702 zirconium is used in chemical plants in valves, pipes, heat exchangers and pumps. These systems are, for example, apparatus for the production of acetic acid, hydrochloric acid or urea. Even in the medical field Zr702 is used because it is biocompatible and shows no toxic effects. Another application of zirconium 702 is the nuclear technology. | |
Welding | Matching welding consumables should be used. Quality 4.8 of welding gases (eg argon with a purity of 99.998%) are recommended. |