General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.7 g/cm³ Show Supplier Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 200 [-] Show Supplier Material materials with Dureza Brinell of 200 [-] | max. |
Elongación A5 | 23.0 °C | 15 % Show Supplier Material materials with Elongación A5 of 15 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 300 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 300 MPa | min. |
Módulo elástico | 23.0 °C | 220 GPa Show Supplier Material materials with Módulo elástico of 220 GPa | |
Resistencia a la tracción | 23.0 °C | 480 - 680 MPa Show Supplier Material materials with Resistencia a la tracción of 480 - 680 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Supplier Material materials with Calor específico of 440 J/(kg·K) |
Conductividad térmica | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 7E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 7E-7 Ω·m |
Magnético
Property | Value |
---|---|
Magnetic properties | Magnetisation is possible |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cromo | 16 - 18 % Show Supplier Material materials with Cromo of 16 - 18 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Molibdeno | 0.8 - 1.4 % Show Supplier Material materials with Molibdeno of 0.8 - 1.4 % | |
Niobio | 1 % Show Supplier Material materials with Niobio of 1 % | max., (min: 4x(C+N)+0.1) |
Nitrógeno | 0.04 % Show Supplier Material materials with Nitrógeno of 0.04 % | max. |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Annealing | 800-860°C | |
Application areas | Automotive Industry, Fasteners, Home appliances, Electronic equipment, Plant construction, Architecture & Decoration | |
General machinability | Good | |
Polishing ability | Very good | |
Welding | TIG welding: suitable, MAG Solid wire: suitable, Arc welding: suitable, UP welding: limited, Laser beam welding: suitable, Gas fusion welding: limited. An extra thermal treatment is not necessary. | |
Workability | Hot forming: 800-1100°C |