General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 440 [-] Show Supplier Material materials with Dureza Brinell of 440 [-] | max. |
Elongación A5 | 23.0 °C | 10 % Show Supplier Material materials with Elongación A5 of 10 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 720 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 720 MPa | min. |
Módulo elástico | 23.0 °C | 200 GPa Show Supplier Material materials with Módulo elástico of 200 GPa | |
Resistencia a la tracción | 23.0 °C | 930 - 1200 MPa Show Supplier Material materials with Resistencia a la tracción of 930 - 1200 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Supplier Material materials with Calor específico of 440 J/(kg·K) |
Conductividad térmica | 23.0 °C | 11 W/(m·K) Show Supplier Material materials with Conductividad térmica of 11 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 7.7E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 7.7E-7 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cobre | 2.5 - 4.5 % Show Supplier Material materials with Cobre of 2.5 - 4.5 % | |
Cromo | 15 - 15.5 % Show Supplier Material materials with Cromo of 15 - 15.5 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Niobio | 0.15 - 0.49 % Show Supplier Material materials with Niobio of 0.15 - 0.49 % | Nb+Ta |
Níquel | 3.5 - 4.5 % Show Supplier Material materials with Níquel of 3.5 - 4.5 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Power Engineering, Plant construction, Chemistry Offshore | |
Corrosion properties | Good | |
Welding | Good |