General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.1 g/cm³ Show Supplier Material materials with Densidad of 8.1 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 250 [-] Show Supplier Material materials with Dureza Brinell of 250 [-] | max. |
Elongación A5 | 23.0 °C | 40 % Show Supplier Material materials with Elongación A5 of 40 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 300 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 300 MPa | min. |
Módulo elástico | 23.0 °C | 195 GPa Show Supplier Material materials with Módulo elástico of 195 GPa | |
Resistencia a la tracción | 23.0 °C | 650 - 850 MPa Show Supplier Material materials with Resistencia a la tracción of 650 - 850 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Supplier Material materials with Calor específico of 450 J/(kg·K) |
Conductividad térmica | 23.0 °C | 12 W/(m·K) Show Supplier Material materials with Conductividad térmica of 12 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1E-6 Ω·m |
Magnético
Property | Value |
---|---|
Magnetic properties | Magnetisation very low |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | max. |
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % | max. |
Cobre | 0.5 - 1.5 % Show Supplier Material materials with Cobre of 0.5 - 1.5 % | |
Cromo | 19 - 21 % Show Supplier Material materials with Cromo of 19 - 21 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Molibdeno | 6 - 7 % Show Supplier Material materials with Molibdeno of 6 - 7 % | |
Nitrógeno | 0.15 - 0.25 % Show Supplier Material materials with Nitrógeno of 0.15 - 0.25 % | |
Níquel | 24 - 26 % Show Supplier Material materials with Níquel of 24 - 26 % | |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Technological properties
Property | ||
---|---|---|
Annealing | 1120-1180°C | |
Application areas | Environmental Technology, Power engineering for onshore and offshore, Chemical & petrochemical, Ship building industry, Medical technology & pharmacy, Cellulose and textile industry, Architecture & Decoration | |
Corrosion properties | Very good/excellent resistance against pitting corrosion | |
General machinability | Very hard | |
Polishing ability | Good | |
Welding | TIG welding: suitable, MAG Solid wire: suitable, Arc welding: suitable, UP welding: suitable, Laser beam welding: suitable, Gas fusion welding: suitable. It has a tendency to hot crack formation. | |
Workability | Hot forming: 950-1200°C |