General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 12 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 12 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 7.8 GPa Show Supplier Material materials with Módulo de flexión of 7.8 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 220 MPa Show Supplier Material materials with Resistencia a la flexión of 220 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 181 MPa Show Supplier Material materials with Resistencia a la tracción of 181 MPa | ASTM D638 |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Auto parts, power tools, wipers | |
Fillers | 30% Glass Fiber |