General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.3 g/cm³ Show Supplier Material materials with Densidad of 1.3 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 58 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 58 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 11.38 GPa Show Supplier Material materials with Módulo de flexión of 11.38 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 11.48 GPa Show Supplier Material materials with Módulo elástico of 11.48 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 280 MPa Show Supplier Material materials with Resistencia a la flexión of 280 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 220 MPa Show Supplier Material materials with Resistencia a la tracción of 220 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Temperatura de flexión bajo carga | 261 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 261 °C | ASTM D648 | |
Inflamabilidad | UL 94 V0 |
Technological properties
Property |
---|