General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 - 3 % Show Supplier Material materials with Elongación of 2 - 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 106 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 15.23 GPa Show Supplier Material materials with Módulo de flexión of 15.23 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 320 MPa Show Supplier Material materials with Resistencia a la flexión of 320 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 201 MPa Show Supplier Material materials with Resistencia a la tracción of 201 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de flexión bajo carga | 220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | ASTM D648 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+15 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.2 % Show Supplier Material materials with Contracción of 0.1 - 0.2 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Carbon Fiber |