General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.51 g/cm³ Show Supplier Material materials with Densidad of 1.51 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 84 [-] Show Supplier Material materials with Dureza Shore D of 84 [-] | ASTM D785 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 80 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 11.4 GPa Show Supplier Material materials with Módulo de flexión of 11.4 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 170 MPa Show Supplier Material materials with Resistencia a la flexión of 170 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de flexión bajo carga | 264 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 264 °C | ASTM D648 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive bumpers, Automotive applications, Automotive exterior parts | |
Fillers | 20% Glass Fiber |