General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 1 - 3 % Show Supplier Material materials with Elongación of 1 - 3 % | ASTM D638 | ||
Impact strength, Charpy notched, ASTM | 23.0 °C | 640 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 640 J/m | ASTM D256 | ||
Módulo de flexión | 23.0 °C | 17.2 GPa Show Supplier Material materials with Módulo de flexión of 17.2 GPa | ASTM D790 | ||
Resistencia a la flexión | 23.0 °C | 305 MPa Show Supplier Material materials with Resistencia a la flexión of 305 MPa | ASTM D790 | ||
Resistencia a la tracción | 23.0 °C | 234 MPa Show Supplier Material materials with Resistencia a la tracción of 234 MPa | ASTM D638 | ||
Resistencia a desgarros | 97.0 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.1 - 0.2 % Show Supplier Material materials with Contracción of 0.1 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Steaming tray, bell-shaped cover, microwave bowl, oven utensils | |
Fillers | 30% Carbon Fiber |