General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 75 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 75 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 6.3 GPa Show Supplier Material materials with Módulo de flexión of 6.3 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 205 MPa Show Supplier Material materials with Resistencia a la flexión of 205 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 136 MPa Show Supplier Material materials with Resistencia a la tracción of 136 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 - 0.6 % Show Supplier Material materials with Contracción of 0.3 - 0.6 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Auto parts, power tools, household electrical appliances | |
Fillers | 25% Glass Fiber |