General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.48 g/cm³ Show Supplier Material materials with Densidad of 1.48 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 20 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 20 J/m | ASTM D256 |
Resistencia a la flexión | 23.0 °C | 260 MPa Show Supplier Material materials with Resistencia a la flexión of 260 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 176 MPa Show Supplier Material materials with Resistencia a la tracción of 176 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Temperatura de flexión bajo carga | 210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | ASTM D648 | |
Inflamabilidad | UL 94 HB (1.6mm) |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 17 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 17 kV/mm | ASTM D147 |
Surface resistivity | 23.0 °C | 1.00E+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+12 Ω/sq | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Additives | Halogen-Free Flame Retardant | |
Application areas | Auto parts, power tools, wipers | |
Fillers | 45% Glass Fiber |