General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 35 % Show Supplier Material materials with Elongación of 35 % | Minimum, ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 60 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 60 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 1.8 GPa Show Supplier Material materials with Módulo de flexión of 1.8 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la flexión of 60 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 48 MPa Show Supplier Material materials with Resistencia a la tracción of 48 MPa | ASTM D638 |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | ASTM D147 |
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Additives | Toughening Additive | |
Application areas | Wheels, electrical shell, automotive parts, rollers, sports equipment |