General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 7.5 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 7.5 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3 GPa Show Supplier Material materials with Módulo de flexión of 3 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 82 MPa Show Supplier Material materials with Resistencia a la flexión of 82 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Temperatura de flexión bajo carga | 220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | ASTM D648 | |
Inflamabilidad | UL 94 V0 (1.6mm) |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.2 - 1.3 % Show Supplier Material materials with Contracción of 1.2 - 1.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Brominated flame retardant Additive |