General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.24 g/cm³ Show Supplier Material materials with Densidad of 1.24 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 91 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 91 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 2.76 GPa Show Supplier Material materials with Módulo de flexión of 2.76 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 172 MPa Show Supplier Material materials with Resistencia a la flexión of 172 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 86.2 MPa Show Supplier Material materials with Resistencia a la tracción of 86.2 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ASTM D648 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+12 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.3 % Show Supplier Material materials with Contracción of 0.2 - 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Flame Retardant |