General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.34 g/cm³ Show Supplier Material materials with Densidad of 1.34 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 210 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 210 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 1.93 GPa Show Supplier Material materials with Módulo de flexión of 1.93 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 62.1 MPa Show Supplier Material materials with Resistencia a la flexión of 62.1 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 41.4 MPa Show Supplier Material materials with Resistencia a la tracción of 41.4 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL 94 V0 (1.5mm) |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Supplier Material materials with Contracción of 0.5 - 0.7 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Flame Retardant |