General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.63 g/cm³ Show Supplier Material materials with Densidad of 1.63 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 8.27 GPa Show Supplier Material materials with Módulo de flexión of 8.27 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 152 MPa Show Supplier Material materials with Resistencia a la flexión of 152 MPa | ASTM D790 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 165 °C Show Supplier Material materials with Temperatura de fusión of 165 °C | ASTM D2117 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | ASTM D147 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |