General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.7 g/cm³ Show Supplier Material materials with Densidad of 1.7 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 75 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 75 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 10.3 GPa Show Supplier Material materials with Módulo de flexión of 10.3 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 159 MPa Show Supplier Material materials with Resistencia a la flexión of 159 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 117 MPa Show Supplier Material materials with Resistencia a la tracción of 117 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.8E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.8E-4 1/K | |
Temperatura de flexión bajo carga | 166 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 166 °C | ASTM D648 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | ASTM D147 |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber |