General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.24 g/cm³ Show Supplier Material materials with Densidad of 1.24 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 82 [-] Show Supplier Material materials with Dureza Shore D of 82 [-] | ASTM D785 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 5.63 GPa Show Supplier Material materials with Módulo de flexión of 5.63 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 78 MPa Show Supplier Material materials with Resistencia a la tracción of 78 MPa | ASTM D638 |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |