General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1 % Show Supplier Material materials with Elongación of 1 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 7.58 GPa Show Supplier Material materials with Módulo de flexión of 7.58 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 117 MPa Show Supplier Material materials with Resistencia a la flexión of 117 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 82.7 MPa Show Supplier Material materials with Resistencia a la tracción of 82.7 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Temperatura de flexión bajo carga | 110 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 110 °C | ASTM D648 | |
Inflamabilidad | UL 94 HB (1.6mm) |
Technological properties
Property | ||
---|---|---|
Fillers | 10% Carbon Fiber |