General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.47 g/cm³ Show Supplier Material materials with Densidad of 1.47 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 130 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 130 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 9.65 GPa Show Supplier Material materials with Módulo de flexión of 9.65 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 228 MPa Show Supplier Material materials with Resistencia a la flexión of 228 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 183 MPa Show Supplier Material materials with Resistencia a la tracción of 183 MPa | ASTM D638 |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1.00E+15 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+15 Ω·m |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Scooter, bearing, fender, bumper, water tank, car handle, bicycle, fuel tank, frame, refrigerator housing, etc | |
Fillers | 40% Glass Fiber |