General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 65 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 65 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3.5 GPa Show Supplier Material materials with Módulo de flexión of 3.5 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 158 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 158 °C | ASTM D648 | |
Inflamabilidad | UL94 HB |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | car bumper,Tube,switch box, fan motor cover, refrigerator back cover, motor support cover, TV shell, refrigerator lining, drawer, soymilk machine cover, electric kettle shell etc | |
Fillers | 30% Glass Fiber |