General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 112 [-] Show Supplier Material materials with Dureza Shore D of 112 [-] | ASTM D785 |
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 96 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 96 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 6.89 GPa Show Supplier Material materials with Módulo de flexión of 6.89 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 93 MPa Show Supplier Material materials with Resistencia a la flexión of 93 MPa | |
Resistencia a la tracción | 23.0 °C | 68.5 MPa Show Supplier Material materials with Resistencia a la tracción of 68.5 MPa |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 3.00E+16 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.00E+16 Ω·m | |
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | ASTM D147 |
Technological properties
Property | ||
---|---|---|
Application areas | car bumper,Tube, switch box, fan motor cover, refrigerator back cover, motor support cover, TV shell, refrigerator lining, drawer, soymilk machine cover, electric kettle shell etc | |
Fillers | 40% Glass Fiber |