General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4 % Show Supplier Material materials with Elongación of 4 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 108 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 108 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 6.14 GPa Show Supplier Material materials with Módulo de flexión of 6.14 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 170 MPa Show Supplier Material materials with Resistencia a la flexión of 170 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | ASTM D638 |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value |
---|---|---|
Surface resistivity | 23.0 °C | 1.00E+16 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+16 Ω/sq |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.8 - 1.1 % Show Supplier Material materials with Contracción of 0.8 - 1.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | LED lamp Housing,Switch, socket etc | |
Fillers | 20% Glass Fiber |