General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.52 g/cm³ Show Supplier Material materials with Densidad of 1.52 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | ASTM D638 | ||
Impact strength, Charpy notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 90 J/m | ASTM D256 | ||
Resistencia a la flexión | 23.0 °C | 335 MPa Show Supplier Material materials with Resistencia a la flexión of 335 MPa | ASTM D790 | ||
Resistencia a la tracción | 23.0 °C | 245 MPa Show Supplier Material materials with Resistencia a la tracción of 245 MPa | ASTM D638 | ||
Módulo de flexión | ASTM D790 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D648 | |
Inflamabilidad | UL94 HB |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.2 - 0.4 % Show Supplier Material materials with Contracción of 0.2 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Handles of surgical equipment, fixtures, prostheses, medical light reflectors, dental appliances etc | |
Fillers | 30% Glass Fiber |