General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.21 g/cm³ Show Supplier Material materials with Densidad of 1.21 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 150 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 5.5 GPa Show Supplier Material materials with Módulo de flexión of 5.5 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 150 MPa Show Supplier Material materials with Resistencia a la flexión of 150 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 108 MPa Show Supplier Material materials with Resistencia a la tracción of 108 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.1 - 0.5 % Show Supplier Material materials with Contracción of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | PA12 is widely used in automobile fuel delivery pipes, automobile brake pipes, air conditioning pipes, pneumatic equipment hoses, industrial high-pressure hydraulic pipes, pipe quick connectors, solenoid shafts, precision gears, cams and bearings, wipers,Car cooling fan, car water tank, car engine bracket etc | |
Fillers | 30% Glass Fiber |