General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Shore D | 23.0 °C | 72 [-] Show Supplier Material materials with Dureza Shore D of 72 [-] | ASTM D785 | ||
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | ASTM D638 | ||
Impact strength, Charpy notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 150 J/m | ASTM D256 | ||
Módulo de flexión | 23.0 °C | 6.21 GPa Show Supplier Material materials with Módulo de flexión of 6.21 GPa | ASTM D790 | ||
Resistencia a la flexión | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la flexión of 179 MPa | ASTM D790 | ||
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | ASTM D638 | ||
Resistencia a desgarros | 12.0 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 178 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 178 °C | ASTM D648 | |
Inflamabilidad | UL94 HB |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 16 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 16 kV/mm | ASTM D147 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic plugs, auto parts, mechanical parts, ships, aerospace, electronic housing etc | |
Fillers | 30% Glass Fiber |