General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Shore D | 23.0 °C | 110 [-] Show Supplier Material materials with Dureza Shore D of 110 [-] | ASTM D785 | ||
Elongación | 23.0 °C | 85 % Show Supplier Material materials with Elongación of 85 % | ASTM D638 | ||
Resistencia a la tracción | 23.0 °C | 47 MPa Show Supplier Material materials with Resistencia a la tracción of 47 MPa | ASTM D638 | ||
Módulo de flexión | ASTM D790 | ||||
Resistencia a desgarros | 47.0 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 178 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 178 °C | ASTM D648 | |
Inflamabilidad | UL94 HB |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic plugs, auto parts, mechanical parts, ships, aerospace, electronic housing etc | |
Fillers | 20% Glass Fiber |