General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.98 g/cm³ Show Supplier Material materials with Densidad of 0.98 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 59 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 59 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 2.35 GPa Show Supplier Material materials with Módulo de flexión of 2.35 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 34.5 MPa Show Supplier Material materials with Resistencia a la tracción of 34.5 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 130 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 130 °C | ASTM D648 | |
Inflamabilidad | UL94 HB |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 1.2 - 1.8 % Show Supplier Material materials with Contracción of 1.2 - 1.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | auto parts,bumer etc | |
Fillers | 20% Talc |