General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Shore D | 23.0 °C | 103 [-] Show Supplier Material materials with Dureza Shore D of 103 [-] | ASTM D785 | ||
Impact strength, Charpy notched, ASTM | 23.0 °C | 58 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 58 J/m | ASTM D256 | ||
Resistencia a la flexión | 23.0 °C | 47 MPa Show Supplier Material materials with Resistencia a la flexión of 47 MPa | ASTM D790 | ||
Resistencia a la tracción | 23.0 °C | 41 MPa Show Supplier Material materials with Resistencia a la tracción of 41 MPa | ASTM D638 | ||
Módulo de flexión | ASTM D790 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.6 - 0.8 % Show Supplier Material materials with Contracción of 0.6 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Air conditioner deflector, signal lamp cover | |
Fillers | 40% Talc |